DAE have one of those days where the mortar sets before you even tap the first brick?
Had a bad one last Tuesday on a job in Rochester, about 90 degrees by 10am and my mud was going off in under 8 minutes. Lost two batches of type S before I smartened up and mixed it thinner and smaller, and my helper kept running it back to the wheelbarrow. By quitting time I'd only laid about 300 block, which is half what I should do in a day. I think the heat plus mixing too much at once got me, but I'm wondering if the sand was off too. Anyone else get burned by fast-setting mud in the heat, and what do you do to stretch the working time?